superalloys

 
英 [suːpə'rælɔɪz]     美 [suːpə'rælɔɪz]    
  • 高温合金

superalloys的用法和样例:

例句

  1. The deviation of preferred orientation of single crystal superalloys from the axis is one of the most important defects.
    摘要单晶高温合金晶体取向与轴向的偏离已成为单晶叶片的一个重要缺陷。
  2. The recrystallization tendency of single crystal superalloys with different levels of carbon at different solution temperatures and compressive stresses was investigated.
    摘要研究了不同碳含量镍基单晶高温合金在不同固溶温度和压应变条件下的再结晶倾向性。