In addition, the coverage and number of carbon layers in CCA can be easily controlled by changing the sucrose content in the precursors and the impregnation times. 在這種複合材料中,碳層厚度可控制為一個石墨單層的厚度,且碳的覆蓋度及層數可以通過改變浸漬的蔗糖量及浸漬次數來進行調控。