The results show that the tensile properties of composite after 100 thermal cycles is 493 MPa, 20% higher than that of as cast composite (411 MPa).

 
  • 结果表明:经过100次热循环后复合材料的拉伸强度为493MPa,比铸态复合材料411MPa提高了20%25;