The results and fractographic observations suggested that the acceleration in crack growth under cathodic polarization was due to hydrogen-induced cracking(HIC).

 
  • 断口显微分析结果显示,阴极极化下加速裂纹的扩展是由于氢致腐蚀(HIC)。