The as-built columns suffered shear failure at low strength and displacement ductility.Shear strength and hysteretic responses of the retrofitted columns were improved significantly.

 
  • 试验结果表明,未加固柱的抗剪强度和延性都比较低,加固后柱的抗剪承载力显著提高,变形性能明显改善。