- The effect of inverted two-stage aging on microstructure and properties of a Ni base superalloy has been studied. 研究了固溶+两段时效热处理工艺对镍基高温合金组织及性能的影响。
- A Ni base superalloy columnar preform were produced through nitrogen spray atomization and deposition. 利用氮气雾化喷射沉积技术成功地获得了宇航用变形镍基高温合金柱形坯。
- The effect of laser shock processing on the microstructure, hardness and residual stress of an austenitic steel 1Cr18Ni9Ti and a Ni base superalloy GH30 is studied as a functions of laser shock processing variables. 利用激光冲击强化技术分别对奥氏体不锈钢 1Cr18Ni9Ti和镍基高温合金 GH30进行了表面强化处理 ;观察了激光表面强化处理后 1Cr18Ni9Ti和 GH30显微组织与结构的变化 ;测定了1Cr18Ni9Ti和 GH30的显微硬度和残余应力 .
- PREDICTION OF CREEP-RUPTURE STRENGTH OF WROUGHT Ni BASE SUPERALLOYS USING ARTIFICIAL NEURAL NETWORK 人工神经网络预测变形高温合金的持久强度
- Surface grain refinement of turbine blades in Ni based superalloy K18 were studied by comparison of experimental results in different alloys and mold surface materials. 选用K18合金和纯金属镍及不同的面层细化料,通过实验对比研究了镍基高温合金叶片表面晶粒细化机理。
- Keywords Ni base superalloy;VIM;deoxidation;denitrogenation; 镍基高温合金;真空感应熔炼;脱氧;脱氮;
- Ni base superalloy 镍基高温合金
- Ni base superalloy K44 镍基高温合金K44
- cast Ni base superalloy 镍基高温合金
- An infrared absorption method for the determination of trace sulfur in nickel base superalloys was presented. 应用红外碳硫测定仪,对镍基高温合金中痕量硫的测定方法进行了研究。
- The wear-resistant dispersion-eleetroplated layer is composed of high-hardness particles distributed on a Ni base. 耐磨分散电镀可以赋予零件表面以镍基体上分布着高硬度微粒的镀层,从而有效地提高耐磨性。
- Keywords Ni based superalloy;melt superheating;microstructure;stress rupture property; 镍基高温合金;熔体过热;显微组织;持久性能;
- The dendritic morphologies of a Ni base single crystal superalloy in , and orientations were observed by optic microscope. 用光学显微镜观察了沿 [0 0 1],[0 11]和 [111]方向生长的镍基单晶高温合金的枝晶形态。
- The influence of the electrode potential on the corrosion behavior of a series of nickel base superalloys has been studied in a 90(mol.%)Na_2SO_4-10 (mol.%) K_2SO_4 melt at 900 C. 研究了在900℃的90Na_2SO_4-10K_2SO_4(克分子%25)熔盐中,电极电位对镍基高温合金腐蚀行为的影响。
- Experimental Study of the Casting Technological Factors on the Surface Microstructure of Grains of Turbine Blade Castings in Ni Based Superalloy 工艺参数对铸件表面显微组织影响的实验研究
- Therma fatigue behaviors of Ni base alloy chromium carbide composite coating made by a vacuum fusion sintering method are discussed in this paper. 研究了用真空熔烧法制得的镍基合金-碳化铬复合涂层的热疲劳行为。
- Study on a Nickel Base Superalloy FGH95 of Turbine Disc? 镍基粉末高温合金FGH95涡轮盘材料研究
- Typical application: Co-WC powder, chrome oxide powder, Lead sesquioxide powder, Chromium carbide powder, zirconium oxide powder, Ni Base Alloy-Chromium Carbide,etc. 典型应用:钴碳化钨粉、氧化铬粉、三氧化二铅粉、碳化铬粉、氧化锆粉、镍铬碳化铬粉、钴铬铌钇粉等。
- Abstract: Therma fatigue behaviors of Ni base alloy-chromium carbide composite coating m ad e by a vacuum fusion sintering method are discussed in this paper. 摘 要: 研究了用真空熔烧法制得的镍基合金-碳化铬复合涂层的热疲劳行为。
- The high-temperature plasma entered through the breach and melted the supporting materials such as Al alloy and Fe,Ni base alloy, which result in the space shuttle Colum... 对于航空、航天与核动力领域中广泛采用的通用关键材料,应该加强其制备工艺的研究,特别是可视化铸造技术的研究。