After electron beam welding,electron beam local heat treatment was applied in GH4133 superalloy as the turbine disk material in this paper.

 
  • 针对涡轮盘材料GH4133合金,在电子束焊后采用新颖的电子束局部热处理工艺对接头进行热处理。