您要查找的是不是:
- He was beaten out with fatigue when he got home. 他回到家里时已是疲惫不堪。
- She fell out from extreme fatigue. 她由于极度疲劳而掉队了。
- A very funny joke may relieve you of a whole day's fatigue. 一则非常滑稽的笑话可以使你消除一天的疲劳。
- The aeroplane wing showed signs of metal fatigue. 机翼显出有金属疲劳的现象。
- fatigue fractography 疲劳断口
- The fractography of the fatigue crack initiation displayed cleavage f... 裂纹形成的断裂为穿晶解理机制,预应变可导致更多的二次裂纹。
- Fatigue is incidental to a journey in a strange land. 在陌生的地方旅行,容易疲劳。
- Causing fatigue or boredom; wearisome. 累人的引起疲劳或厌烦的; 使人疲劳的
- It is a treat to have a drink after the fatigue of the day. 干了一天的累活後喝杯酒其乐无穷。
- Finally, her mind gave in to fatigue and she fell asleep. 最后她的心力疲惫不堪,就睡着了。
- The bending fatigue properties and fractography of normalized tufftrided 45 steel were analyzed. 对45钢正火态软氮化处理前后的旋转弯曲疲劳性能及其断口进行了定量和电镜分析。
- The fractography of the fatigue crack initiation displayed cleavage facet and more second cracks after pre-training. 裂纹形成的断裂为穿晶解理机制,预应变可导致更多的二次裂纹。
- He hasn't got over his fatigue yet. 他的疲劳还没有恢复。
- Keywords: fractography, brittle material, failure mode, model rock. 关键词:裂形学、脆性材料、破裂模式、人工岩石。
- Causing physical or mental fatigue; tedious or tiresome. 乏味的使体力或智力疲倦的; 乏味的或令人厌倦的
- His thoughts drooped with fatigue. 他的思维由于疲乏而丧失了活力。
- Working overtime caused him great fatigue. 加班加点地工作使他疲惫不堪。
- Fractography analyses with scanning electronic microscopy (SEM) were conducted to determine fatigue fracture mechanisms of these two lead-free solders. 此外,亦利用扫描式电子显微镜(SEM)观察表面裂缝与疲劳破断面,以了解此两款无铅焊锡之疲劳破裂机制。
- Cage layer fatigue is a type of osteoporosis. 笼养蛋鸡疲劳症是骨质疏松症的一种类型。
- His eyes were bleary with fatigue. 他累得双眼昏花。
- 今日热词
-
- 深远海浮式风电平台 - deep-sea floating wind power platform
-
- 京雄高速公路 - Beijing-Xiongan expressway
-
- 农业及相关产业增加值 - the added value of agriculture and related industries