When the contents of KH550-treated attapulgite and EOC-g-MAH is 10% and 15% respectively,compared with crude EOC,100% tensile modulus,tensile strength and tear strength of AT/EOC composites increase by 104%,65%,25% respectively.

 
  • 当经KH5 5 0处理的凹凸棒石为 10份 ,接枝率为 0 89%25的EOC g MAH为 15份时 ,复合材料的 10 0%25拉伸模量、拉伸强度和撕裂强度分别比EOC弹性体提高 10 4%25、65%25、2 5%25。