When composite inhibitors (VC and Cr_3C_2) are doped with 0.4wt% individually, they can effectively inhibit WC crystal growth and hardmetal with excellent properties can be obtained.

 
  • 当复合抑制剂VC+Cr_3C_2的加入量分别为0.;4%25wt时,抑晶效果最佳,硬质合金性能达到最优;