When Mo content is 10%,the synthetical properties of the Ti-Mo alloy are the best. The data of hardness(4510 MPa),compression strength(1636 MPa),compression ratio(22.5%) and elastic modulus(29.8 GPa) were collected.

 
  • Mo含量为10%25;合金的综合性能最好:硬度为4510 MPa;压缩强度为1636 MPa;压缩率为22.;5%25;弹性模量为29