The wormhole-like mesostructure can retard the collapse rate of mesopores through grain growth during crystallization.

 
  • 又因虫洞状孔洞仍存留于长大之晶粒内,阻碍氧化钨晶粒成长,提高孔洞崩解温度与热稳定性。