The results showed that the untreated PTW were corroded in acid solution at pH 2.0 and dissolved by boiling concentrated sulfuric acid.

 
  • 未处理的PTW在pH=2.;0的酸性溶液中开始被腐蚀;并能被煮沸的浓硫酸所溶解;