The results showed that attaked surface had similar appearance like impact fractograph primary failure mechanism of cavitation damage was mixed mode of quasi cleavage and dimple fracture.

 
  • 观察结果表明 ,其剥落形貌与冲击断口形貌相似 ,剥落机制主要是韧窝和准解理的混合型。