The results show: the addition of shrinkage reducing agent(SRA) reduced the early shrinkage significantly,especially in first 7 days.

 
  • 通过自由收缩、质量损失、强度、平板抗裂性等试验研究减缩剂(SRA)的减缩抗裂效果。