The effective band width more than 10 dB of the sample reaches 6.2 GHz and the highest absorption peak is 34 dB when the thickness of sample is 2 mm,the frequency is in the range of 2? 18 GHz,Sr content is 0.2 and Fe content is 0.12 and 0.14,respectively.