您要查找的是不是:
- A surface defect in paper. Alternative terms: blisters; foam marks. 中义纸张的表面缺陷,参考字:气泡痕迹。
- Surface defect and macrostructure of high carbon steel billet were analyzed. 介绍了铸坯相关表面缺陷及低倍组织,提出了质量控制措施及方案。
- Exterior measurement includes specification and size, surface defect, and sewing requirement. 外观质量包括规格尺寸及公差、表面疵点、缝制要求。
- Zinc content in the alloy above 0. 05% consistently resulted in an unacceptable surface defect as galvanizing. 锌含量低于0.05%25时,型材一般不发生雪花状腐蚀。
- Surface defect detection is important to ensure the utility,integrality,and security of the products. 产品表面缺损检测对保证产品的使用性能、完整性和安全性具有重要意义。
- The article describes the problem of the toughened glass' surface defect and the method of prevention and solution. 针对钢化玻璃表面质量存在的变形点缺陷,采取相对应措施预防和解决。
- Small and superficial occlusal surface defect ,proximal and labial surface defect uninvolved incisal angle . 2 .;合面缺损范围小而且表浅,前牙邻、唇面缺损未涉及切角者,不宜用嵌体修复。
- Using flexible interpolator pad is an important way to suppress the part surface defect in stretch-farming process on multi-paint tool. 摘要采用柔性垫层是抑制和消除多点模拉形过程中零件表面缺陷的重要措施。
- This paper analyzes the reason that caused the surface defect of billet produced by EAF Steelmaking plant of Nanjing Iron and Steel Co.Ltd. 分析了南(京)钢电炉厂小方坯表面质量问题及产生的原因,涉及结晶器振动参数、保护渣等。
- Objective: To provide anatomic basis for repairing the knee joint surface defect with the pedicled patella translocation. 摘要目的:为带血管蒂髌骨移位修复股骨髁和胫骨髁关节面缺损提供解剖学基础。
- Using flexible interpolator pad is an important way to suppress the part surface defect in stretch-forming process on multi-point tool. 采用柔性垫层是抑制和消除多点模拉形过程中零件表面缺陷的重要措施。
- The results show that 82B wire rod brittle fracture is mainly caused by excessive inclusion,reticulate carbide,lower sorbite in the microstructure,and surface defect of wire rod. 结果表明,82B钢盘条脆断的主要原因是夹杂物级别超标、组织中出现网状碳化物、索氏体含量偏低以及盘条表面缺陷等。
- Surface defect in cold rolled galvanization plate in Handan Iron and Steel Limited Group has been introduced,meanwhile the solution process has been discussed. 介绍邯钢冷轧热镀锌线在生产中所遇到的一些表面缺陷,及对解决过程中所遇到的一些问题进行探讨。
- The main shortages in MnSi surface and the reasons are analysed,the measures to improve MnSi surface quality and to reduce the loss by the surface defect are put forword. 分析了锰硅合金表面质量的主要缺陷及其产生的主要原因,提出了改善锰硅合金表面质量,减少因表面质量缺陷而造成损失的措施。
- On the basis of the rigid viscoplastic FEM theory, a surface defect prediction method for the plastic forming process by FEM numerical simulation has been thoroughly studied. 摘要基于刚粘塑性有限元基本理论,本文深入地研讨了通过有限元数值模拟来预测塑性成形问题中一类表面缺陷生成的方法。
- The effect of molten steel purity, casting temperature, performance of protecting slag, oscillation and liquid level control of mold in continuous casting on surface defect wa. 重点阐述了钢水洁净度、浇铸温度、保护渣性能、结晶器振动以及液面控制等连铸工艺对表面质量的影响。
- The process of refinishing parts that have a surface defect from the first coat. Application of a second coat after correction of the defect in the first coating. 把第一次涂装存在缺陷的工件重新涂装的过程,应用第二次涂装来修复第一次涂装时的缺陷。
- The surface defect appeared mainly as air bubbles and ferroferric oxide drops which centred around the lower outer - field portion of the stoneware cup. 表观缺陷主要表现为釉泡和氧化铁颗粒,且其集中于杯体下部外侧面。
- Surface defects on this ABS part were caused by an improperly shaped gate. 这个ABS工件的表面缺陷由浇口的形状设计不当引起。
- The surface defects decrease the nanowire's energy transport capability. 当纳米线表面存在缺陷时,其热传导系数小于无缺陷纳米线的值。