Mechanical properties after T4 and T6 tempering got marked improvement as AZ91D can be solution and aging strengthened while vacuum assisted die casting gave it this opportunity.

 
  • 热处理后(T4和T6),由于AZ91D具有固溶强化和时效强化效果, 合金的性能相对于压铸态有大幅度的提高。