It is found that traveling block hook was brittle fracture and crack originated from original flaw per Macro fractography and micro fractography.

 
  • 对游车大钩断裂事故进行了调查研究,对其断口形貌进行了宏观和微观分析,发现游车大钩为脆性断裂,断口起源于原始缺陷。