Crack spreading area and transient breaking are observed, typical fatigue striations, fatigue steps and secondary cracks are observed on some of the fractures.

 
  • 微观上在少数油管断口中观察到了典型的疲劳辉纹,在很多断口上观察到了疲劳台阶和二次裂纹。