After 10 h ball milling,the alloy of carbonyl iron and carbonyl nickel began to form,and the sample kept its original bcc and fcc structure;

 
  • 球磨10 h时,羰基铁和羰基镍开始形成合金,但大部分Fe、Ni原子仍分别以bcc结构和fcc结构存在。